SikaBond® SBR+ | SBR Bonding

Mixing procedures for topping and screeds containing Sikabond® SBR+ are similar to those used to conventional compositions, with gauging water partly replaced by Sikabond® SBR+. However, mixing time should be minimised to limit air entrainment. Mixing should be carried out in a forced action mixer. The usual procedure is to pre-mix sand and cement in the mixer, pour in the Sikabond® SBR+, mix for 1 - 3 mins, then slowly add water to the required consistency.
NB. Over-addition of water causes rapid thinning of latex modified mortars owing to the plasticising effect of the latex. The mix design depends upon thickness and intended use. However, typically mixes for a 12 mm topping or screed are as follows:

Link to HAOZE

If you want to learn more, please visit our website Styrene Butadiene Latex for Bitumen.

Additional reading:
Where to order custom fit floor mats and trunk liners

                           Screed            Topping
O.P.C                     1                      1
Moist sand           3.5                   1.75
3 mm Washed

Want more information on NBR Latex for safety gloves? Feel free to contact us.

Comments

0 of 2000 characters used

All Comments (0)
Get in Touch

  |   Transportation   |   Toys & Hobbies   |   Tools   |   Timepieces, Jewelry, Eyewear   |   Textiles & Leather Products   |   Telecommunications   |   Sports & Entertainment   |   Shoes & Accessories   |   Service Equipment   |   Sitemap